Two frames can leave the same workshop with the same silhouette and still feel completely different in the hand. The difference is almost always the surface finish. On a metal frame, polishing, electroplating and PVD coating are not cosmetic extras bolted on at the end of production — they are the steps that decide how the frame reflects light, how it resists perspiration and humidity, and whether the colour still looks intentional after a year of daily wear. This guide follows each stage in the order it happens on the line, then looks at how coating adhesion and durability are checked before a run is released.
A metal frame is judged long before anyone examines the hinge or the temple tips. The eye reads the surface first: whether reflections are continuous or broken, whether edges look soft or cut, whether the colour reads as a deliberate finish or as a layer sitting on top of the metal. A well-finished frame hides the marks of its own manufacturing — the weld joint, the tool marks, the transition where a temple meets a rim. A poorly finished one exposes all of them.
Finishing also carries the functional load. Base metal needs a barrier between itself and the skin, and that barrier is the plating or the coating. If the barrier is thin, porous or weakly bonded, the frame fails at the surface even though the geometry is perfectly correct.
Everything that follows depends on this step. A coating can only be as smooth and as well bonded as the surface beneath it, so polishing is where a large part of final quality is actually decided.
Production usually begins with barrel polishing, where frames are tumbled with abrasive media. It is efficient for removing grinding marks, rounding sharp edges and reaching a uniform semi-bright surface across many pieces at once. Barrel type, media shape and cycle time are chosen according to the alloy and the target finish.
Where the geometry is delicate, or where the finish needs to be brighter than a barrel can deliver, hand polishing takes over. A skilled polisher works the rims, bridge and temple profiles with buffing wheels and progressively finer compounds. This is the stage that removes the last visible tool marks and builds the lustre that a mirror finish depends on.
Between stages, frames are cleaned. Polishing compounds and buffing residue are oily, and they will contaminate a plating bath or interfere with coating adhesion, so degreasing and rinsing sit between polishing and coating rather than after it. Inspection at this point looks for residual scratches, burn marks from over-buffing, distortion of thin sections, and any area the wheel could not reach.
Electroplating deposits a metal layer onto the frame by passing current through an electrolyte. The frame acts as the cathode, dissolved metal ions deposit onto its surface, and the deposit follows the surface it grows on — which is exactly why polishing quality shows through.
Most metal eyewear is plated in more than one layer. A typical sequence builds a base layer for adhesion and corrosion performance, then one or more colour or brightening layers on top. Common finishes include nickel-based systems, chrome for a bright silver look, gold and gold-toned deposits, and darker tones such as gunmetal or black. For frames intended for sensitive skin, nickel-free or nickel-reduced systems are often specified in place of conventional nickel underlayers.
What matters at the plating stage:
Physical vapour deposition works differently. Instead of depositing from a liquid electrolyte, PVD runs inside a vacuum chamber. A source material is vaporised — by evaporation or by sputtering — and the vapour condenses onto the frames as a thin film. Because the process is line-of-sight inside the chamber and the frames are rotated through the cycle, coverage on complex shapes depends heavily on fixture design.
PVD is usually chosen for reasons electroplating cannot fully cover:
The trade-off is process discipline. PVD bonds to a clean surface or it does not bond at all. Any trace of polishing compound, mould release, oxide or handling oil becomes a localised adhesion failure. Pre-treatment — ultrasonic cleaning, drying, and in some cases a thin intermediate layer — is therefore not optional, and chamber load, vacuum quality and cycle parameters need to stay consistent from run to run.
Adhesion tests are deliberately simple, because the failure modes are simple. The logic is always the same: cut through the coating, apply a pull, and see whether the film stays with the substrate.
Acceptance criteria are agreed between buyer and supplier and written into the specification. What matters at production scale is not the result of a single test piece but consistency across the run. Samples are therefore taken from different positions in the plating rack or the PVD chamber load, because adhesion problems are often positional rather than random.
In service, a metal frame meets three things repeatedly: skin contact, moisture and abrasion. Durability testing tries to reproduce those conditions in a compressed way.
As with adhesion, results are read against agreed criteria rather than against an absolute figure, and testing is repeated across production lots so that a drifting bath or a contaminated chamber is caught in the factory rather than at the customer.
Buyers who get consistent finishing usually make the requirements explicit instead of leaving them implied. Useful items to state:
Being specific here removes the ambiguity that most often turns into a finish complaint: both sides assuming the other understood which test, which sample and which acceptance level applied.
Polishing, electroplating and PVD coating do different jobs, but they are one continuous process. Polishing establishes the surface. Plating or PVD builds the barrier and the colour. Adhesion and durability testing verify that what was built will survive the way the frame is actually worn. A supplier who treats these as a single chain — and who tests for adhesion and durability rather than only for appearance at the end of the line — is the one producing frames that still look right after a year of use, not just on the day they ship.